Draft 1 on a 20-25µm texture: 0.7mm less travel, double ejection force
Draft angle should not be a single number handed to every wall. A bare wall needs 0.5-1 degree. A...
Tag archive
Draft angle should not be a single number handed to every wall. A bare wall needs 0.5-1 degree. A...
Boss cracking is mostly a wall-ratio failure. The working numbers: boss wall thickness is 0.5-0.6...
A weld line's position is decided by the gate; its depth is decided by melt and mould temperature....
Mold cost for an enclosure splits into three tiers, and choosing the wrong tier is not a one-off...
Paint-free molding does not save paint. It saves the paint line: fixtures, paint and labour, rework...
A snap-fit that feels loose, or one that cannot be pressed home, is almost never a design mistake in...
A color approved on a paper chip is not a color yet. It is an intention. Between the chip and the...
A customer sent us a 3D file from a mold that had already run. The only request was to swap PC/ABS...
A batch of small-appliance housings came back from the tool shop: matte top cover, gloss bottom...
Whether an appearance design can actually ship comes down to something plain: can the factory make...
Start with the answer. A set of exterior 3D files bought from an appearance-styling studio usually...
Start with the number. Draft angle = base 1–1.5° + (actual texture depth ÷ 0.025 mm) × 1°. A 0.02 mm...